The use of inoculants that contain low, controlled levels of bismuth and lanthanum increase the nucleation, nodule count, in ductile irons.
Use of these powerful inoculants provides for greater chill reduction in thin sections, and increased nodule count in all section sizes. If enhanced nucleation is required, this potent inoculant may be the tool to use.
Silicon
Bismuth
Tre
Calcium
Aluminum
60.00-70.00%
1.00-1.50%
0.60-1.00%
1.00-1.50%
0.60-1.00%
Size :
3/8″ x 20 mesh (2mm x 10mm)
20 mesh x 80 mesh (0.2mm x 0.7mm)
Effective Date :
1/25/17