Miller and Company is a leading supplier of alloys used in iron foundry applications. Our broad range of alloys includes Nodulizers, Inoculants, Ferro-Alloys, Moly-Oxide, Copper, Tin, Antimony, pure Magnesium, Nickel and Iron Pyrites. Miller offers exothermic risers, and Cored Wire is available with any Ferro-Alloy or specialty alloy.

Dependable and reliable sourcing is assured through our international network. In addition, all steel foundry alloys are subject to Miller's rigorous certification and quality assurance program, to ensure consistent properties and exacting chemistries. Stock is maintained at conveniently located warehouses throughout North America.

Typical Analysis and Sizes
Aluminum
  % Al            
Chops 99.5 min            
Antimony
 
% Sb            
  99.0 min            
Calcium
  % Si % Ca % Ba % Mn % Al    
Calcium Silicon 52-65 30-33 - - 2.00 max    
Calcium Silicon
Barium
50-60 14-18 14-18 - 2.00 max    
Chromium
  % Cr % C % Si % P      
Charge Chromium (A) 51-56 6-8 6.0 max. 0.03 max.      
Charge Chromium (B) 56-62 6-8 8.0-14.0 max. 0.03 max.      
Ferro-Chrome  
High Carbon 62-72 6-8 3.00 max 0.03 max      
High Carbon
(Low Si)
62-72 6-8 0.80 max 0.03 max      
Low Carbon
(0.015% C Grade)
65-72 0.015 max 1.00 max 0.03 max      
Low Carbon
(0.025% C Grade)
65-72 0.025 max 1.00 max 0.03 max      

Low Carbon
(0.05% C Grade)

65-72 0.05 max 1.00 max 0.03 max      
Low Carbon
(0.10% C Grade)
65-72 0.10 max 1.00 max 0.03 max      
Low Carbon
(0.15% C Grade)
65-72 0.15 max 1.00 max 0.03 max      
Low Carbon
(0.20% C Grade)
65-72 0.20 max 1.00 max 0.03 max      
Copper
  % Cu            
Chops Grade 1 99.9 min            
Chops Grade 2 96.0 min            
Shot 99.3 min            
Inoculation Products
For Gray and Ductile Iron % Si % Ca % Ba % Sr % Al % Ti % Mg
75% FeSi-CAB 70-79 0.80-1.80 - - 1.60 max  - -
75% FeSi-Ca+Ba 70-79 0.8-1.5 0.8-1.5 - 1.50 max - -
IM 75B 70-79 0.80-1.30 0.80-1.30 - 0.75 - 1.20  - -
IM SR 70-79 0.10 max - 0.80-1.20 0.50 max  - -
IMTI-LC 50-55 0.50 -1.50 - - 0.90-1.30 10.0-12.0 -
MG1 46-50 0.80-1.20 - - 1.20 max - 1.00-1.50
TENBLOC 60-75 0.4-1.50 0.15-0.40 0.3-0.75 0.6-5.0 - -
Magnesium
  % Mg            
Pure Magnesium Metal 99 min            
Manganese 
Ferromanganese % Mn % C % Si % P      
(Std.) High Carbon 74-82 7.50 max 1.20 max 0.35 max      
Low Phosphorus 77-79 7.50 max 1.20 max 0.10 max      
Medium Carbon 80-85 1.50 max 1.50 max 0.30 max      
Low Carbon 85-90 0.75 max 2.00 max 0.30 max      
Mischmetal
  % TRE % Ce % La % Nd % Pr Other
R.E.M.
 
Mischmetal 98.0 48.0 20.0-32.0 12.0-20.0 5.0-8.0 3%  
Silico Manganese
  % Mn % Si % C % P  % S    
Silico Manganese 65-68 16-18.50 2.0 max 0.20 max 0.04 max    
Molybdenum
  % Mo % C % Si % S % P    
Ferro-Molybdenum 60-70 0.10 max 2.00 max 0.15 max 0.05 max    
MgFeSi
Treatment Alloys for Ductile Iron % Si % Mg % Ce % TRE % Al % Ca  
MG 5R-2 43-48 5.85-6.50 - 0.80-1.20 1.20 max 0.8-1.3  
MG 5R-2-HCA 43-50 6.00-6.50 - 0.80-1.20 0.8-1.2 1.60-2.20  
MG 4R 43-48 4.00-4.50 - 1.50-2.00 1.20 max 0.80-1.30  
MG1 46-50 1.00-1.50 - - 1.20 max 0.80-1.20  
Phosphorus
Ferro-Phosphorus % P % Si % Mn % C      
Ferro-Phosphorus 22-26 3.0 max 3.0 max 0.25 max      
Lo Sil Ferro-Phos.
Briquette
22-25 (Not
retained)
3.0 max 0.05 max      
Rare Earth Silicide
  % TRE % Ce % Si % Ti % Al % Ca % Fe
Rare Earth Silicide

30.0-33.0

14.0-16.0 35.0-39.0 0.8 max 1.5 max 2.0 max Balance
Silicon
Ferro-Silicon % Si % Al          
50% Regular 47-51 1.25 max          
75% Regular 74-79 1.50 max          
Sulfur
  % S          
Iron Pyrites 53.2 ± 2%
Typical
           
Iron Pyrites Briquettes 50% Typical            
 Tin
  % Sn            
Shot / Bars 99.0 min            
Titanium
  % Ti % C % Al % Si       
Ferro-Titanium 65-75 0.30 max 4.50 max 0.25 max          
IMTI-LC 10-12 0.50-1.50 0.90-1.30 50.0-55.0